Product Name : Concrete Crack Grouting Adhesive
Product Specifications : 20kg/bucket
Shelf Life : 12 months
Construction Temperature : 5–45°C








Concrete cracks are physical structural changes caused by the interaction of internal and external factors within a concrete structure. Cracks are a major cause of reduced load-bearing capacity, durability, and waterproofing in concrete structures. Different treatment methods are typically used for different types of cracks.
1 : Epoxy Resin Crack Filler System: A two-component modified epoxy low-viscosity liquid adhesive, characterized by low viscosity, low heat release, long pot life, and simple filling process.
2 : Epoxy resin filler: This sealant can be injected into micro-cracks as wide as 0.1mm, exhibiting good aging resistance and resistance to various media (acids, alkalis, water).
3 : It contains no volatile solvents and does not shrink during curing.
4 : It possesses excellent toughness and impact resistance after curing.
5 : With formula adjustments, it can be used for underwater crack filling.
|
Performance Items |
|
|
|
Physical Properties |
Specific Gravity, g/cm3 |
0.9~1.0 |
|
Pot Life,min |
>30 |
|
|
Curing Time,天: |
<7 |
|
|
Colloid Properties |
Tensile Strength, MPa |
>20 |
|
Compressive Strength,MPa |
>50 |
|
|
Tensile Modulus of Elasticity, MPa |
1500 |
|
|
Bonding Properties |
SteeltoSteel Shear Strength,MPa |
>10 |
|
Aging Resistance |
90d,Steel-steel shear strength reduction rate≤10% |
|
|
Environmental Performance |
This product complies with Limits of Harmful Substances in Adhesives for Interior Decoration and Refurbishment Materials |
|
Transportation hubs, roads, bridges and tunnels, water conservancy and hydropower, ports and waterways, energy bases, municipal construction, etc.